electrical:batterycide [2017/11/09 18:25] frater_secessus [murdering flooded lead-acid] |
electrical:batterycide [2018/06/30 20:58] frater_secessus [murdering flooded lead-acid] |
| |
===== murdering flooded lead-acid ===== | ===== murdering flooded lead-acid ===== |
Flooded lead-acid (FLA) batteries are the most resillient to mistreatment but they can be killed. | Flooded lead-acid (FLA) batteries are the most resillient to mistreatment but they too can be killed. |
| |
* leaving them at [[electrical:12v:psoc|partial state of charge]], resulting in //irreversible// sulfation | * leaving them at [[electrical:12v:psoc|partial state of charge]], resulting in //irreversible// sulfation((AKA "hard" sulfation. The battery undergoes "soft" sulfation and desulfation during normal charging/discharging.)) |
* not charging soon enough; they need charging every day | * not charging soon enough; fully charging each day is best. |
* not charging fully; they need a [[electrical:12v:charging#absorption_stage|long Absorption stage]] at manufacturer-recommended voltage to reverse normally-occurring ("soft") sulfation.((http://support.rollsbattery.com/support/solutions/articles/5964-battery-sulfation)) \\ [[electrical:generator#charging_batteries|Generator-only charging]] can cause this unless the generator runs the necessary number of hours it takes to complete Absorption. \\ Less commonly, [[electrical:solar|Solar]]-only charging can cause this problem if the [[electrical:solar:sizing|battery capacity is too great for the solar output]]. | * not charging fully; they need a [[electrical:12v:charging#absorption_stage|long Absorption stage]] at manufacturer-recommended voltage to reverse normally-occurring ("soft") sulfation.((http://support.rollsbattery.com/support/solutions/articles/5964-battery-sulfation)) \\ [[electrical:generator#charging_batteries|Generator-only charging]] can cause this unless the generator runs the necessary number of hours it takes to complete Absorption. \\ Less commonly, [[electrical:solar|Solar]]-only charging can cause this problem if the [[electrical:solar:sizing|battery capacity is too great for the solar output]]. |
* discharging too deeply. Maximum discharge should be 50% [[electrical:depth_of_discharge|depth of discharge]]. | * discharging too deeply. Maximum discharge should be 50% [[electrical:depth_of_discharge|depth of discharge]]. |